Howard Evans's Album: Accelerated Thermal Fatigue Test

(1) Dip a specially coated tool-steel rod into molten aluminum, then (2) lift it out and (3) dip it into water. (4) Lift it out of water and (5) blow dry. Repeat from (1) until coating fails or 2000 dip cycles, whichever occurs first.

Photo 2 of 6 in Accelerated Thermal Fatigue Test

Aluminum Melting Furnace
Almost assembled furnace (with spare insulation segments on right in photo), but without aluminum end caps and 1/4-20 Allthread support rods attached.